Reciclado de baterías de ión-Li agotadas. Aplicaciones 1. Introducción tecnológicas de los metales recuperados
Before leaching the powder was calcined at 750 oC and characterized by XRD, DRIFT and SEM-EDS. Using a S/L = 30 g L-1, 2 h, 5 vol% H2O 2, at 30 oC and in one step, 93-99% Li, 90-91% Mn, 80-84% Ni and 88-91% Co was extracted. After leaching, a mixed Mn-Ni-Co hydroxide with composition Ni0.43Mn0.28Co0.29(OH) was.